Rdzenie ferrytowe UY




|
MODEL |
OSTRY |
WAGA |
ROZMIAR (mm) |
PARAMETR |
WAGA (g) |
|||||||||||
|
A |
Prędkość obrotowa |
C |
D |
E |
F |
C1mm-1 |
Lemm |
Emm2 |
Vmm3 |
|||||||
|
UYF12,5/3570 |
Ⅱ |
100 |
36.0±0.6 |
12.5 |
9.9±0.2 |
12.5±0.2 |
24.8±0.2 |
34.8±0.2 |
1.33 |
159.6 |
119.8 |
19127 |
93.5 |
|||
|
UYF12/3670 |
Ⅱ |
93 |
36.5±0.8 |
15.8 |
|
8.3±0.3 |
12.0±0.3 |
25.0±0.3 |
35.0±0.3 |
1.56 |
166.0 |
106 |
17640 |
85 |
||
|
UYF13/3560 |
Ⅲ |
91 |
35.0±0.6 |
11.8 |
9.9±0.3 |
12.9±0.3 |
20.8±0.3 |
30.8±0.3 |
1.10 |
140.1 |
126.3 |
17505 |
85 |
|||
|
UYF13/3566 |
Ⅲ |
94 |
35.0±0.6 |
11.8 |
9.9±0.3 |
12.9±0.3 |
22.5±0.3 |
32.5±0.3 |
1.14 |
140.1 |
126.4 |
18101 |
88 |
|||
|
UYF13/3660 |
Ⅱ |
92.5 |
35.7±0.6 |
12.5 |
9.7±0.3 |
12.9±0.3 |
20.8±0.3 |
30.8±0.3 |
1.14 |
144.1 |
126.3 |
18205 |
87.5 |
|||
|
UYF15/4268 |
Ⅲ |
142 |
41.2±0.8 |
14.5 |
12.0±0.3 |
14.9±0.3 |
22.5±0.3 |
34.2±0.3 |
0.93 |
160.6 |
171.2 |
27498 |
134 |
|||
|
UYF15/4275 |
Ⅲ |
152 |
41.2±0.8 |
14.5 |
12.0±0.3 |
14.9±0.3 |
25.5±0.3 |
37.5±0.3 |
1.00 |
174.6 |
174.4 |
30462 |
141 |
|||
|
UYF16/4376 |
Ⅱ |
176 |
43.0±0.8 |
14.5 |
12.0±0.3 |
15.9±0.3 |
26.0±0.3 |
38.0±0.3 |
0.91 |
175.5 |
192.2 |
33734 |
164 |
|||
|
UYF17/4677 |
Ⅱ |
206 |
46.2±0.8 |
15 |
16.7±0.3 |
13.3±0.3 |
25.6±0.3 |
38.5±0.3 |
0.85 |
212.0 |
180 |
38236 |
195 |
|||
|
UY10/3244 |
Ⅳ |
44.6 |
32.0±0.6 |
12.5 |
10.0±0.2 |
\ |
14.0±0.3 |
22.0±0.3 |
1.45 |
108.9 |
75.1 |
8178 |
42 |
|||
|
UY12/4257 |
Ⅳ |
78 |
41.5±1.0 |
19 |
11.7±0.3 |
\ |
19.0±0.4 |
28.5±0.3 |
1.37 |
148.5 |
108.2 |
16000 |
68 |
|||
|
UY12/4035 |
Ⅳ |
57 |
39.0±1.0 |
16 |
11.7±0.3 |
\ |
6.8±0.3 |
17.6±0.3 |
1.12 |
96.4 |
85.4 |
8240 |
52 |
|||
|
UY16/5858 |
Ⅳ |
167 |
58.0±0.8 |
25.5 |
|
16.0±0.2 |
\ |
17.0±0.3 |
29.0±0.3 |
0.84 |
164.8 |
194.7 |
32098 |
148 |
||
|
UY16/5860 |
Ⅳ |
169 |
58.0±0.8 |
25.5 |
16.0±0.2 |
\ |
18.0±0.3 |
30.0±0.3 |
0.86 |
167.0 |
195.1 |
32584 |
151 |
|||
|
UY16/6060 |
Ⅳ |
173 |
60.0±0.8 |
27.5 |
16.0±0.3 |
\ |
18.0±0.3 |
30.0±0.3 |
0.88 |
171.0 |
194.9 |
33335 |
150 |
|||
|
UY16/6062 |
Ⅳ |
177 |
60.0±0.8 |
27.5 |
16.0±0.2 |
\ |
19.0±0.3 |
31.0±0.3 |
0.90 |
175.1 |
195.1 |
34161 |
153 |
|||
|
UY74 powiedział: |
Ⅳ |
256 |
72.5±1.5 |
37.8 |
17.6±0.4 |
\ |
19.0±0.5 |
35.3±0.5 |
0.83 |
207.0 |
250.6 |
51938 |
230 |
|||
|
UY22 |
Ⅳ |
646 |
101.0±2.0 |
55 |
22±0.5 |
\ |
33.0±0.6 |
51.0±0.6 |
0.79 |
307.0 |
388 |
120000 |
581 |
|||
|
UY30 |
Ⅳ |
1198 |
98.0±2.0 |
40 |
29.0±0.5 |
\ |
41.5±0.5 |
66.0±0.5 |
0.48 |
330.8 |
691.9 |
228500 |
1054 |
|||
|
UY34 powiedział: |
Ⅳ |
3160 |
121±2.0 |
38 |
42.0±1.0 |
\ |
55.5±0.5 |
89.7±0.5 |
0.30 |
422.8 |
1419 |
600000 |
2781 |
|||
|
UY42 |
Ⅳ |
3160 |
121±2.0 |
38 |
42.0±1.0 |
\ |
55.5±0.5 |
89.7±0.5 |
0.30 |
422.8 |
1419 |
600000 |
2781 |
|||
|
UR22A |
Ⅰ |
420 |
55.0±2.0 |
20 |
22.0±0.5 |
35.8±0.5 |
28.0±0.4 |
40.0±0.4 |
0.49 |
195.0 |
400 |
78000 |
370 |
|||
|
UR22B |
Ⅰ |
332 |
52.0±1.5 |
17 |
22.0±0.5 |
32.0±0.5 |
20.0±0.4 |
32.0±0.4 |
0.43 |
162.0 |
374 |
60625 |
292 |
|||
|
UR22C |
Ⅰ |
266 |
45.7±1.0 |
11.2 |
22.0±0.5 |
32.0±0.5 |
14.0±0.4 |
26.0±0.4 |
0.34 |
125.5 |
370 |
46400 |
234 |
|||
Popularne Tagi: rdzenie ferrytowe uy, Chiny producenci, dostawcy, fabryki rdzeni ferrytowych uy
Wyślij zapytanie